PLA · Budget PLA

Inland PLAPLAFilament Review & Print Settings

4.2/5

Micro Center house brand PLA. Popular US budget option.

Quick Specs

Brand
Inland
Material
PLA
Print temp
195-225°C
Bed temp
50°C
Speed
55 mm/s
Cost/kg
$18

Colors Available

BlackWhiteRedBlueGreenGreyYellow

Print Settings Guide for Inland PLA

PLA is the friendliest material in FDM printing and Inland PLA is no exception. Set your nozzle between 195-225°C — start at the lower end to minimize stringing, raise it if you see underextrusion or layer delamination. A bed temperature of 50°C with PEI or glass gives excellent first-layer adhesion. No enclosure needed — PLA performs well in open-air environments at room temperature. Print speed can be aggressive: most PLA handles 55 mm/s without quality loss. Use fan cooling at 100% after the first layer to keep bridges clean and overhangs sharp. Retraction between 1–6mm (direct: 0.5–2mm, Bowden: 4–7mm) controls stringing on this material.

Why Choose Inland PLA

Inland PLA has earned solid community respect for consistent diameter tolerances, reliable color accuracy across batches, and predictable print behavior. Inland is known for tight ±0.02–0.05mm tolerance control, which means fewer jams and more consistent flow rates. PLA's biodegradable plant-based chemistry also makes it a responsible choice for hobbyists who print high volumes. Reviews across 3D printing communities consistently highlight low odor, good layer bonding, and reliable first-layer adhesion as standout strengths of this type of filament.

What to Print with Inland PLA

Inland PLA excels at decorative objects, figurines, cosplay props, tabletop terrain, desktop organizers, and educational models. PLA's detail resolution is among the best of common FDM materials — fine features at 0.4mm line widths are achievable with good cooling. Prototype parts that don't face heat or significant mechanical stress are a natural fit. Architectural models, scale miniatures, and custom keychains are all classic PLA projects. For anything that will live outdoors or near a hot car window, consider PETG or ASA instead — PLA softens around 60°C.

Common Issues & Fixes

Stringing: drop nozzle temp by 5°C and increase retraction. Warping on large flat prints: first layer temp +5°C, slow first layer to 25 mm/s, use a brim. Poor bed adhesion: clean bed with IPA before every print — skin oils destroy adhesion. Elephant foot: lower initial layer flow to 90-95%. Brittle prints after storage: PLA absorbs moisture slowly; dry at 45°C for 4 hours before printing if stored over 6 months.

Notes

Micro Center exclusive. Budget champion with decent reliability.

Where to Buy Inland PLA

Find Inland PLA from Amazon and authorized resellers. Price comparison helps — filament costs vary by vendor, fulfillment location, and quantity. Check manufacturer storefronts for direct pricing and bundle deals.

PrintLog3D participates in the Amazon Associates program. Purchases through our links may earn a small commission at no extra cost to you.

Log your PLA prints in PrintLog3D

Track your actual settings for Inland PLA — nozzle temp, bed adhesion, slicer profile, and results. Build a settings history that tells you exactly what works.